Selecting Tungsten Carbide Grades for Punches, Dies & Mold Inserts

Start with what limits tool life. A drawing die that gradually loses bore accuracy and a stamping punch that chips at one corner call for different grade reviews. Locate the wear or damage and check the working geometry, fit, support, and operating conditions before changing the carbide grade.

How to compare carbide grades

In tungsten carbide–cobalt (WC–Co) grades, finer carbide grains generally increase hardness at comparable cobalt content. At comparable grain size, more cobalt generally increases fracture toughness and reduces hardness. Use these trends to shortlist candidates, then compare supplier data and experience with similar tools and operating conditions.

  • Hardness measures resistance to indentation. It helps screen grades for abrasive duty when considered alongside the actual wear mechanism. Compare values measured on the same scale and, for Vickers hardness, at the same test load.
  • Transverse rupture strength (TRS) is the bending stress at which a test specimen breaks under specified conditions. Compare results obtained with the same test method and specimen geometry.
  • Fracture toughness describes resistance to crack extension. Compare values obtained by the same method, and review any separately reported impact test data when shock loading is a concern.

Use the Tooling, Die & Mold grade tables to shortlist grades for heading, stamping, and powder compaction. Confirm the required properties and acceptance criteria for the specific component before ordering.

Cold heading

Cold-heading punches and die inserts must retain their working profiles under repeated forming loads. If a tool chips early, locate the origin of the damage and review alignment, support, and the amount of deformation at the affected stage. If the setup is sound and fracture still limits tool life, compare grades with greater fracture toughness and relevant cold-heading experience. If the profile wears gradually, compare grades that offer better wear resistance while withstanding the forming loads. 
View carbide grades for cold and hot heading

Drawing

For wire, bar, and tube drawing dies, inspect the reduction zone and sizing land. Compare bore diameter, roundness, and surface condition with the drawing and with measurements of the drawn product. Check the workpiece material and surface condition, reduction per pass, lubrication, and die profile.

Finer-grained grades can be candidates where abrasive bore wear limits die life. If grooves or product marks are accompanied by material pickup, check adhesion and lubrication before using hardness to rank grades. If the die cracks or chips, also review the insert fit, support, and process loads. Use product size and surface finish as acceptance criteria in a production trial.

Extrusion

For cold extrusion, assess the forming loads, working profile, and support of the insert. If it cracks or chips, review contact and loading around profile transitions before comparing tougher grades. If gradual wear changes the extruded profile, compare grades that can retain the working geometry under those loads.

For warm or hot extrusion, include the expected tool temperature and thermal cycling. Review the effect of temperature on fit if the carbide insert is installed in a steel holder. Ask for grade data or application experience at relevant temperatures so the selection accounts for the conditions the tool will see in service.

Progressive stamping

Review the sheet material and thickness, punch-to-die clearance, alignment, and wear pattern at each station. A gradual increase in burr height warrants an inspection of both cutting edges for rounding or wear. Localized chipping calls for a check of clearance, alignment, stock feeding, and support at the affected station.

For electrical steel laminations, cold-rolled steel, copper, and aluminum, use the motor lamination and sheet stamping or precision progressive stamping grade table as appropriate to the operation. Compare candidates using burr height, cut-edge condition, dimensional consistency, and strokes between regrinds. If workpiece material builds up on the tool, also review its surface finish and lubrication. 
• View carbide grades for motor laminations and sheet stamping
• View carbide grades for precision progressive stamping

Mold cores and cavity inserts

Start with the molded material, the required surface finish, and the features that must hold tolerance over repeated cycles. For abrasive filled materials, identify where wear occurs and compare grades for their ability to retain the specified profile and finish. If process materials or cleaning agents may attack the binder, assess compatibility using the actual chemistry, concentration, temperature, and exposure time.

For a replacement core or cavity insert, provide the approved drawing and the relevant dimensions of the existing mold. Inspect the insert seat and adjacent mating surfaces for wear or damage that could affect fit and alignment.

Powder compaction

For compaction punches and die inserts, consider powder abrasiveness, part geometry, pressing and ejection loads, and working surface condition. Inspect the areas of highest wear and check whether ejection loads or inadequate support are contributing to chipping. Where corrosion is a concern, review binder compatibility using the powder formulation and operating conditions.

When pressing magnetic powders such as ferrite or NdFeB, confirm whether the die components have a magnetic property requirement. EnduraCarbide offers WZ09 and WZ15 as non-magnetic carbide grades for these applications. If the specification sets a magnetic permeability limit, provide that limit and the applicable test method for the grade review. 
View carbide grades for powder compaction

What to provide for a grade review

  • The approved component drawing, including working geometry, tolerances, finish, and relevant mating dimensions.
  • The workpiece material or powder formulation, the operation, and relevant conditions such as lubrication, load, speed, and temperature.
  • The current carbide grade if known, service life in cycles or parts, and the reason the tool was removed from service.
  • Photos showing the location of the damage, along with part measurements and the tool feature that changed.

Agree on the trial acceptance criteria before switching grades. Compare candidates under equivalent production conditions and record both tool life and part quality. For example, track strokes to the burr-height limit in stamping or parts produced before a bore-size or surface-finish limit is reached in drawing.